Manufacturers introduce the factors that affect the wear of the dosing device

During the operation of the automatic dosing device, after the material is crushed, the particle size of the stone begins to decrease, but at the same time, due to the high hardness of the material, the steel product receives damage and wear. Below we will have a detailed understanding of the factors affecting the wear of steel in the dosing device:

*, the loss of steel and medicine of the medicinal mill is related to the size of the steel, the movement of the steel, and the ratio of the steel. Choosing the right parameters can greatly reduce the wear of the steel. Generally, according to the actual work experience, a section of grinding should have a large impact on the ore. Therefore, the impact force should be mainly in the grinding cylinder. The size of the steel should be increased. The second-stage grinding should be fine-grained. The size of the steel should be reduced as much as possible.

Second, the amount of charge has a certain influence on the wear of steel. When other conditions are certain, the charge rate increases within a certain range, which will improve the grinding effect. When the charge rate reaches 50%, the grinding effect is better. In actual production, the charge rate is below 50%. Controlling the charge rate will also improve the grinding effect and reduce the wear of steel. In addition, the wear of steel is also affected by the rotation speed of the mill. As the rotation speed of the mill increases, the movement of the steel is changed from sloping to falling. When the speed is constant, the useful power reaches the large, and then the speed of the mill increases. Will make the steel medicine centrifugal movement, can not get the grinding effect.

Green Prickly Ash

Green Prickly Ash,Pricklyash Peel Green Prickly Ash,Green Peppercorns Prickly Ash,Green Chinese Prickly Ash

Sichuan Liuhang Agriculture Co.Ltd , https://www.lhagriculture.com